The control of the hot-working processes from the initial billet transformation procedures to the final forging of precision components is critical for the generation of consistent mechanical properties.
We supply forgings in nickel-based superalloys that are ideal for demanding applications in the aerospace and power generation industries.
We supply forgings in nickel-based superalloys that are ideal for demanding applications in the aerospace and power generation industries.
Material grades
Grade |
UNS Number |
DIN |
Werkstoff Nr |
---|---|---|---|
Alloy 718 | N07718 | NiCr19Fe19Nb5Mo3 | 2.4668 |
Alloy 718 Plus | |||
Waspaloy | N07001 | NiCr20Co13Mo4Ti3Al | 2.4654 |
Alloy 909 | N19909 | X4NiCo38Nb | |
Alloy 907 | N19907 | X4NiCo38Nb |
SEE MORE
SEE LESS
Alloy 625 | N06625 | NiCr22Mo9Nb | 2.4856 |
Alloy 600 | N06600 | NiCr15Fe8 | 2.4816 |
Alloy 617 | N06617 | NiCr23Co12Mo | 2.4663 |
Alloy X | N06002 | NiCr22Fe18Mo | 2.4665 |
Alloy H230 | N06230 | NiCo29Cr28Si | 2.4880 |
Alloy 188 | R30188 | CoCr22NiW | 2.4683 |
Alloy H242 | N10242 | ||
Alloy HR120 | N08120 | NiFe33Cr25Co | 2.4854 |
Nimonic 80 | N07080 | NiCr20TiAl | 2.4952 |
Alloy 825 | N08825 | NiCr 21 Mo | 2.4858 |
Alloy 800 H | N08800 / N08810 | X8 NiCrAlTi 32-21 | 1.4876 / 1.4958 |
Alloy C276 | N10276 | NiMo 16 Cr 15 W | 2.4819 |
Monel 400 | N04400 | NiCu 30 Fe | 2.4360 |
Alloy C263 | N07263 | NiCo20Cr20Mo6Ti2Al | 2.4650 |
Alloy 286 | S66286 | X5 NiCrTi 26-15 | 1.4980 |
Rene 41 | N07041 | NiCr19Co11MoTi | 2.4973 |
Thermo Span |
ADVANTAGES
Excellent
mechanical
strength at
high temperatures
mechanical
strength at
high temperatures
Creep resistance
under high stress
conditions
under high stress
conditions
High corrosion
& oxidation
resistance
& oxidation
resistance